Material properties of the fasteners

Case hardening steelHeat-treatable steel
  • min. surface hardness 450 HV
  • core hardness 300-350 HV
The tensile strength of these fasteners is at least 900 N/mm², i.e. it corresponds at least to a 9.8 screw.

Yield strength is approx. 90% of tensile strength. Elongation as break is in the range of 10.9 to 12.9 screws.

Threads can be generated in base materials up to 150HB/500 N/mm².
  • 8.8, 9.8, 10.9 and 12.9 qualities

Used in applications with dynamic loads combining tensile stress and bending stress.

Threads can be generated in base materials up to 120HB/ 400 N/mm² (possibly higher if special steps are taken).

Stainless materialsAluminium
  • A2-70/A4-70 for base materials up to
    300 N/mm²
  • A2-70-SX/A4-70-SX for base materials up to 500 N/mm²
  • for special applications